Argenco 333
Reduced Gold Alloys for Crown and Bridge
Color | WHITE |
Type | 4 |
ADA Class | NOBLE (N) |
Application
![]() ![]() ![]() ![]() |
Processing | |
---|---|
Investment | Phosphate Bonded |
Crucible | Graphite / Ceramic |
Degassing Temp C | 650-980 |
Oxidation Procedure |
Solder & Laser Wires | |
---|---|
PreSolder | --- |
PostSolder | LO, R |
Laser Wire |
Physical Properties | |
---|---|
VHN After Firing | |
VHN Soft | 210 |
VHN Hard | 230 |
Proof Stress Soft MPa | 485 |
Proof Stress Hard MPa | 605 |
Tensile Strength Soft MPa | 640 |
Tensile Strength Hard MPa | 725 |
Elongation Soft | 10 |
Elongation Hard | 7 |
Elastic Modulus GPa | 116 |
Composition | |
---|---|
Silver (Ag) | 48.06 |
Copper (Cu) | 16.9 |
Palladium (Pd) | 33.34 |
Zinc (Zn) | 1.6 |
Iridium (Ir) | 0.1 |
Thermal Properties | |
---|---|
Melting Range C | 950-1010 |
Casting Temp C | 1125 |
Density g/cc | 10.6 |
Expansion at 500C | |
Expansion at 600C | |
Burnout Temp C | 705 |