DPM Argenco 62

High Gold Alloys for Crown and Bridge

Color YELLOW
Type 2/3
ADA Class HIGH NOBLE (HN)
Application
Processing
Investment Gypsum or Phosphate Bonded
Crucible Graphite / Ceramic
Degassing Temp C
Oxidation Procedure
Solder & Laser Wires
PreSolder ---
PostSolder 585, 615
Laser Wire LWO75
Physical Properties
VHN After Firing
VHN Soft 130
VHN Hard 220
Proof Stress Soft MPa 262
Proof Stress Hard MPa 324
Tensile Strength Soft MPa 414
Tensile Strength Hard MPa 483
Elongation Soft 50
Elongation Hard 26
Elastic Modulus GPa 76
Composition
Silver (Ag) 26.5
Gold (Au) 62.0
Copper (Cu) 8.99
Palladium (Pd) 1.0
Zinc (Zn) 1.5
Iridium (Ir) 0.01
Thermal Properties
Melting Range C 900-930
Casting Temp C 1010
Density g/cc 14.2
Expansion at 500C
Expansion at 600C
Burnout Temp C 650